Low alloy copper-coated solid wire tig rod designed for welding low alloy steels with 1% Ni content, fine grained for low temperature applications (-50°C).Suitable for the construction of offshore platforms, pressure vessels and pipelines.
| C | 0.10 |
| Si | 0.60 |
| Mn | 1.10 |
| Ni | 1.00 |
| I1 | ||||
| Yield strength | 510 MPa | |||
| Tensile strength | 600 MPa | |||
| Elongation | 26 % | |||
| Impact test Kv (-20°C) | 130 J | |||
| Impact test Kv (-40°C) | 80 J | |||
| Impact test Kv (-50°C) | 70 J |