INETIG B2 L

TIG rods for welding 1.25% Cr. 0.5% Mo. steels

TIG Rod AWS A 5.28: ER70S-B2L EN ISO 21952-B: G 52 M22 1CML with1.25% Cr and 0.5% Mo, for welding heat-resistant steels. heat exchangers, boilers, pipes and pressure vessels up to about 550 ° C. X and J Factor controlled. good mechanical properties
Classifications
  • AWS A 5.28: ER70S-B2L
  • EN ISO 21952-B: W 52 I1 1CML
REQUEST LISTING
DOWNLOAD DOCUMENTS

Low Alloyed TIG Rod with 1.25% Cr and 0.5% Mo, used to weld heat-resistant steels. Also suitable for welding 0.9% Cr and 0.5% Mo steel. Used in the chemical industry and in ammonia synthesis processes, in heat exchangers, boilers, pipes and pressure vessels with operating temperatures up to about 550 ° C. Used in petrochemical plants, Can also be used for carryovers, castings and repair of castings. X and J Factor controlled.

C 0.03
Si 0.60
Mn 0.60
Cr 1.30
Mo 0.50
I1
Yield strength 450 (T) MPa
Tensile strength 560 (T) MPa
Elongation 23 (T) %
Impact test Kv (R.T.) 250 J (T)
  • TUTTE

DOWNLOAD DOCUMENTS

 I have read the privacy policy. (Read policy)