Rutile-coated electrode with low carbon concentration designed for welding stainless steel with 23% Cr and 13% Ni content with service temperature in the range of -80°C and 300°C. Suitable for heterogeneous welding, generally between dissimilar steels, stainless and carbon-manganese steels. It is used for joints and cushion layers for stainless filler metal. Suitable for all positions, very good looking weld bead and easily removable slag.
| C | 0.03 |
| Mn | 1.30 |
| Si | 0.80 |
| Cr | 24.00 |
| Ni | 13.00 |
| Yield strength | 440 MPa | |||
| Tensile strength | 600 MPa | |||
| Elongation | 32 % |
| Diameter (mm) | Length | Ampere |
| 2.0 | 300 | 30-60 |
| 2.5 | 300 | 40-80 |
| 3.2 | 350 | 70-100 |
| 4.0 | 350 | 90-140 |